Preparing sub-micron macroporous ion exchange materials by mechanical grinding, comprises processing product slurry having an average particle size in a stirred ball mill or planetary ball mill at specific process time

Publication: DE102012021559A1
Published: 2014-05-08
Family Size: 1
Granted: No

Simple SummaryContent extracted from patent full text and abstract with AI.

The patent describes a method to produce sub-micron-sized, macroporous ion exchange materials. It involves processing a product slurry with an average particle size below 100 micrometers using mechanical grinding, specifically in a stirred ball mill or planetary ball mill, for a duration of 10 to 180 minutes. This process allows the precise reduction of particle size to the sub-micron scale while maintaining the desired macroporous properties.

Use CasesContent extracted from patent full text and abstract with AI.

  • Manufacturing advanced ion exchange resins for water purification and desalination systems
  • Development of high-performance catalysts for chemical industries
  • Improvement of separation processes in pharmaceutical or biochemical applications
  • Enhancement of battery performance through better electrode materials
  • Wastewater treatment and environmental remediation technologies

BenefitsContent extracted from patent full text and abstract with AI.

  • Achieves sub-micron particle sizes for superior material performance
  • Preserves macroporous structure for enhanced functionality such as higher surface area and improved ion exchange capacity
  • Scalable and controllable process suitable for industrial production
  • Wide applicability across multiple industries and advanced technologies
  • May lower production costs and improve efficiency of ion exchange materials

Technical Classifications (CPCs)

Main Classifications

Manufacturing & Transport

Sub Classifications

Physical & Chemical Processes

Working Plastics & Substances

CPC Codes

B01J43/00B01J47/018B29B13/10

Inventors & Applicants

Applicants

Tech Universität Bergakademie Freiberg

Patent Abstract

Preparing sub-micron macroporous ion exchange materials by mechanical grinding, comprises processing a product slurry having an average particle size of less than 100 mu m in a stirred ball mill or planetary ball mill with process time of 10-180 minutes.

Key Information

Publication No.

DE102012021559A1

Family ID

50489543

Publication Date

2014-05-08

Application No.

DE102012021559A

Application Date

2012-11-02

Priority Date

2012-11-02

Granted

No